สืบค้นงานวิจัย
POROUS PIPE PRODUCTION FOR AGRICULTURE
Sumana Jammeuan - ไม่ระบุหน่วยงาน
ชื่อเรื่อง (EN): POROUS PIPE PRODUCTION FOR AGRICULTURE
ผู้แต่ง / หัวหน้าโครงการ (EN): Sumana Jammeuan
บทคัดย่อ (EN): In this research work, porous pipes were produced from natural rubber (NR), ethylene propylene diene monomer (EPDM) and ground rubber tire (GRT) using dinitrosopentamethylenetetramine (DNPT) as a blowing agent and urea as a kicker. The mixtures were compounded by a two-roll mixing mill, extruded into porous pipe by a single-screw extruder and vulcanized by a hot air oven at 160 °C. Factors affecting porous pipe properties were studied such as NR/EPDM ratio, vulcanization time, % carbon black loading, Rubber/GRT ratio and % blowing agent loading (DNPT). The porous pipe properties were characterized such as tensile strength and water permeation rate. It was found that suitable vulcanization conditions were at 160 °C for 20 min. When carbon black loading was increased, it was found that tensile strength was increased up to an optimum point after which this property deteriorated. As % GRT loading was increased, tensile strength was decreased. Porous pipe compound of NR/EPDM/CB/GRT/DNPT ratio of 80/20/50/150/10 had good properties (tensile strength of 3.7 MPa) and water permeation rate suitable for agricultural applications.
บทคัดย่อ: ไม่พบข้อมูลจากหน่วยงานต้นทาง
ภาษา (EN): en
เผยแพร่โดย (EN): การยางแห่งประเทศไทย
คำสำคัญ (EN): Ground rubber tire
เจ้าของลิขสิทธิ์ (EN): การยางแห่งประเทศไทย
หากไม่พบเอกสารฉบับเต็ม (Full Text) โปรดติดต่อหน่วยงานเจ้าของข้อมูล

การอ้างอิง


TARR Wordcloud:
กระทู้ของฉัน
ผลการสืบค้นทั้งหมด โพสต์     เรียงลำดับจาก